標(biāo)準(zhǔn):
符合GB SAI1070
相當(dāng)AWS ER1100
說明:
S301是含鋁大于99.5%的純鋁焊絲。具有良好的可焊性和耐蝕性,以及優(yōu)良的塑性及韌性,但強(qiáng)度較低。
S301 is pure aluminum welding wire with aluminum content greater than 99.5%. It has good weldability and corrosion resistance, as well as excellent plasticity and toughness, but low strength.
用途:
氬弧焊及氧-乙炔氣焊焊接純鋁及對(duì)接頭性能要求不高的鋁合金作填充材料,廣泛應(yīng)用于化學(xué)工業(yè)鋁制設(shè)備上。
Argon arc welding and oxygen-acetylene gas welding are used as filler materials for pure aluminum and aluminum alloys that do not require high joint performance. They are widely used in aluminum equipment in the chemical industry.
焊絲化學(xué)成分:
Si | Fe | Cu | Mn | Al |
≤0.3 | ≤0.3 | ≤0.04 | ≤0.03 | 余量 |
供應(yīng)規(guī)格(mm):
盤裝Φ | 1.0 | 1.2 | 1.5 | 2.0 | 2.5 | | |
焊絲直徑Φ (長(zhǎng)度1000) | 1.5 | 2.0 | 2.5 | 3.0 | 4.0 | 5.0 | 6.0 |
注意事項(xiàng):
1. 焊前應(yīng)嚴(yán)格清除工件焊接邊緣和焊絲表面的氧化膜和油污等污物,否則會(huì)使焊縫產(chǎn)生熔合不良并引起氣孔、夾渣等缺陷。
2. 為了保證焊透而又不導(dǎo)致塌陷,施焊時(shí)可采用墊板以托住熔化金屬。
3. 氧-乙炔氣焊時(shí)必須配鋁氣焊熔劑共同使用。
1. Strictly remove the oxide film and oil stains on the welding edge of the workpiece and the surface of the welding wire before welding, otherwise it will cause poor fusion of the weld and cause defects such as pores and slag inclusion.
2. In order to ensure penetration without causing collapse, a backing plate can be used to hold the molten metal during welding.
3. Oxygen-acetylene gas welding must be used together with aluminum gas welding flux.